Q.

What is the welding defect caused due to improper control and poor removal of slog between passes called?

  • AMismatch
  • BUnder fill
  • CCrack
  • DPorosity
Correct Answer : (B)

Under fill

Hints :
Previous

Two streams of liquid metal which are not hot enough to fuse properly result into a casting defect known as

Next

In ultrasonic machining, the metal is removed by